I-Industrial High Tenacity Polyamide Nylon N6 Multifilament FDY DTY POY Yarn Fiber
I-Polyamide (PA), evame ukwaziwa nge-Nylon fiber iyifayibha yokwenziwa yokuqala evela emhlabeni futhi iyifayibha yepulasitiki yobunjiniyela be-thermoplastic enezakhiwo ezinhle kakhulu zokusebenza.Ama-molecule enayiloni anamaqembu -CO- kanye -NH-, angakha izibopho ze-hydrogen phakathi noma ngaphakathi kwama-molecule, futhi angahlanganiswa namanye ama-molecule.Ngakho-ke, inayiloni inomthamo omuhle wokumunca umswakama futhi ingakha isakhiwo sekristalu esingcono.
I-Polyamide (PA) Ifayibha enayiloni inokumelana okuhle kwe-alkali, kodwa ukumelana ne-asidi okubi.Ngaphansi kwezinga lokushisa elivamile legumbi, ingakwazi ukumelana no-7% we-hydrochloric acid, u-20% we-sulfuric acid, u-10% we-nitric acid, kanye no-50% we-caustic soda ukuze i-polyamide fiber ifanele izingubo zokusebenza zokulwa nokubola.Ngaphezu kwalokho, ingasetshenziswa njengenetha lokudoba ngenxa yokungagugiki kwamanzi olwandle.Impilo yamanethi okudoba enziwe nge-Polyamide (PA) Inayiloni ifayibha yinde izikhathi ezi-3 kuya kwezi-4 kunamanethi avamile okudoba.
Ngenxa yamandla ayo aphezulu, ukumelana nomthelela kanye nokumelana kahle nokuhuzuka, imayela le-polyamide lezintambo zamasondo enziwe amathayi liphakeme kunalelo lezintambo ezivamile zamasondo e-rayon.Ngemuva kokuhlolwa, amathayi entambo yamasondo e-polyamide angahamba cishe u-300,000km, kuyilapho amathayi entambo yamasondo e-rayon akwazi ukuhamba amakhilomitha angu-120,000 kuphela.Intambo esetshenziswa entanjeni yesondo inezici zamandla aphezulu, i-modulus ephezulu kanye nokumelana nokukhathala.Ngenxa yesibopho samangqamuzana e-polyamide esakhiweni esigoqiwe, inayiloni 66 nenayiloni 6 zingama-polyamides.Amandla wangempela kanye nemodulus yefiber kufinyelela kuphela ku-10% yenani lethiyori.
Amandla okuphuka kwefiber ye-polyamide angu-7~9.5 g/d noma ngisho nangaphezulu, futhi amandla okuphuka kwesimo sawo esimanzi cishe angu-85%~90% walokho esimweni esomile.I-Polyamide (PA) Ifayibha enayiloni inokumelana nokushisa okungekuhle okuphenduka kubephuzi ngemva kwamahora ama-5 ku-150℃ Celsius, iqala ukuthamba ku-170℃ bese incibilika ku-215℃.Ukumelana nokushisa kwenayiloni 66 kungcono kunenayiloni 6. Ukushisa kwayo okuphephile kungu-130 ℃ futhi ngokulandelanayo.90℃.I-Polyamide fiber inokumelana okuhle kwezinga lokushisa eliphansi.Ngisho noma isetshenziswa ekushiseni okuphansi okungu-70 ℃, izinga layo lokululama elinwebekayo alishintshi kakhulu.
Ezisetshenziswa zezimboni, i-polyamide (PA) Inayiloni ifayibha ingasetshenziselwa amanetha okudoba, izindwangu zokuhlunga, izintambo, izindwangu zamasondo amathaya, amatende, amabhande okuthutha, izindwangu zezimboni, njll futhi isetshenziswe ikakhulukazi njengamapharashuthi nezinye izindwangu zempi ekuvikelweni kwezwe.
Kungani ukhetha i-AOPOLY Nylon Yarn?
◎ Umshini: imigqa emi-4 ye-polymerization, amasethi ayi-100 omshini wokusonta oqondile, amasethi angama-41 wama-primary twisters &.i-compound twister, amasethi angama-41 omshini wokweluka indwangu we-Dornier waseJalimane, amasethi ama-2 wemigqa yokucwilisa, ne-Auto Product Flaw Inspection System
◎ Izinto zokusetshenziswa: izinto ezintsha zokusetshenziswa (izinto zasekhaya nezingenisiwe), ama-masterbatches angenisiwe kanye namafutha angenisiwe ukuze akhiqize
◎ Isampula: isampula elinembile linganikezwa izidingo zekhasimende.
◎ Ikhwalithi: ikhwalithi ephezulu ye-oda efana nesampula
◎ Amandla: cishe.100,000tons ngonyaka
◎ Imibala: emhlophe eluhlaza, ephuzi ngokukhanyayo, ephinki
◎ MOQ: 1tons ngombala ngamunye
◎ Ukulethwa: ngokuvamile yizinsuku ezingu-15 ku-40HQ ngemva kokuthola idiphozi
Izicelo Eziyinhloko
Intambo ye-Nylong6 isetshenziselwa kakhulu indwangu yenayiloni, indwangu yenayiloni, indwangu ye-nylon geo, izintambo, inetha lokudoba, njll.
Amapharamitha
Ukucaciswa kweNylon6 Industrial Yarn
Into No | I-AP-N6Y-840 | I-AP-N6Y-1260 | I-AP-N6Y-1680 | I-AP-N6Y-1890 |
Ukuminyana Komugqa (D) | 840D/140F | 1260D/210F | 1680D/280F | 1890D/315F |
Ukuqina ngesikhathi sekhefu (G/D) | ≥8.8 | ≥9.1 | ≥9.3 | ≥9.3 |
Ukuminyana komugqa (dtex) | 930+30 | 1400+30 | 1870+30 | 2100+30 |
I-Coefficient ehlukile yokuminyana komugqa (%) | ≤0.64 | ≤0.64 | ≤0.64 | ≤0.64 |
Amandla okuqina (N) | ≥73 | ≥113 | ≥154 | ≥172 |
Ukwelula ngesikhathi sekhefu (%) | 19-24 | 19-24 | 19-24 | 19-24 |
Ukwelulwa ekulayisheni okujwayelekile (%) | 12+1.5 | 12+1.5 | 12+1.5 | 12+1.5 |
I-Coefficient ehlukile yamandla aqinile (%) | ≤3.5 | ≤3.5 | ≤3.5 | ≤3.5 |
Ukwelulwa kwamandla okuqinile ngesikhathi sekhefu (%) | ≤5.5 | ≤5.5 | ≤5.5 | ≤5.5 |
I-OPU (%) | 1.1+0.2 | 1.1+0.2 | 1.1+0.2 | 1.1+0.2 |
Ukuncipha kwe-Thermal 160 ℃, 2min (%) | ≤8 | ≤8 | ≤8 | ≤8 |
Ukuzinza kwe-Thermal 180℃, 4h (%) | ≥90 | ≥90 | ≥90 | ≥90 |
Ukucaciswa kwe-Nylong6 Industrial Fabric
Ukwakhiwa Kwentambo | |||||
Into No | 840D/2 | 1260D/2 | 1260/3 | 1680D/2 | 1890D/2 |
Amandla okuphuka (N/pc) | ≥132.3 | ≥205.8 | ≥303.8 | ≥269.5 | ≥303.8 |
I-EASL 44.1N (%) | 95+0.8 | ||||
I-EASL 66.6N (%) | 95+0.8 | ||||
I-EASL 88.2N (%) | 95+0.8 | ||||
I-EASL 100N (%) | 95+0.8 | 95+0.8 | |||
I-Adhesion H-Test 136℃, 50min, 3Mpa (N/cm) | ≥107.8 | ≥137.2 | ≥166.5 | ≥156.8 | ≥166.6 |
I-Coefficient ehlukile yamandla okuphuka (%) | ≤5.0 | ≤5.0 | ≤5.0 | ≤5.0 | ≤5.0 |
I-coefficient ehlukile yobude ekuqhekekeni (%) | ≤7.5 | ≤7.5 | ≤7.5 | ≤7.5 | ≤7.5 |
I-Dip pick up (%) | 4.5+1.0 | 4.5+1.0 | 4.5+1.0 | 4.5+1.0 | 4.5+1.0 |
Ukwelula ekuqhekekeni (%) | 23+2.0 | 23+2.0 | 23+2.0 | 23+2.0 | 23+2.0 |
I-Cord gauge (mm) | 0.55+0.04 | 0.65+0.04 | 0.78+0.04 | 0.75+0.04 | 0.78+0.04 |
Ukusonteka kwekhebula (T/m) | 460+15 | 370+15 | 320+15 | 330+15 | 320+15 |
Ukuhlolwa kwe-Shrinkage 160℃, 2min (%) | ≤6.5 | ≤6.5 | ≤6.5 | ≤6.5 | ≤6.5 |
Okuqukethwe umswakama (%) | ≤1.0 | ≤1.0 | ≤1.0 | ≤1.0 | ≤1.0 |
Ububanzi bendwangu (cm) | 145+2 | 145+2 | 145+2 | 145+2 | 145+2 |
Ubude bendwangu (m) | 1100+50 | 1300+50 | 1270+50 | 1300+50 | 1270+50 |